MEMSnet Home: MEMS-Talk: losing features during development
losing features during development
2004-03-18
Kristie A Henchir
2004-03-19
Cain, Mike
2004-03-31
Henchir, Kristie
losing features during development
Kristie A Henchir
2004-03-18
Hi Everyone,

 I am trying to create 15 - 100 micron line widths on a silicon wafer
using AZ4620. The hard part is that I would like the resist thickness to
be around 20 microns. I use the recipe below but find that the smaller
features (15 and 20 microns) delaminate from the wafer during development.
I would appreciate any input/advice you might be able to give regarding
this problem.

1. Clean and dehydrate wafer for 15 min at 120C  2. Spin HMDS at 3000 rpm
for 30 sec (we do not have vapor priming capabilities) 3. Spin AZ4620 at
3000 rpm for 30 sec  4. wait 5 min  5. softbake at 110C for 5 min  6.
spin second layer of resist at 3000 rpm for 30 sec  7. wait 5 minutes   8.
bake for 5 min at 110C  9. wait 1 hour before exposure 10. develop
with AZ 400K diluted 1:4 (development takes 3 minutes)
I appreciate your input.
Sincerely,
Kristie




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation