Hello,

I would like to know if someone has already done anodic bonding with
porous silicon and pyrex. Does it function like si / pyrex anodic
bonding or conditions must be changed?

all the best,

Emeline MERY

Doctorante
Laboratoire de Physique de la Matière (LPM)
UMR CNRS 5511
INSA de Lyon
7 avenue Jean Capelle, bât. Blaise Pascal
69621 VILLEURBANNE CEDEX
FRANCE
Tél. : (33) 4 72 43 87 95
Fax : (33) 4 72 43 60 82




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
MEMStaff Inc.
The Branford Group