MEMSnet Home: MEMS-Talk: Re: Metals for ohmic contact on silicon
Re: Metals for ohmic contact on silicon
2004-03-24
Masa Rao
2004-03-26
MT Klaus Beschorner
Re: Metals for ohmic contact on silicon
MT Klaus Beschorner
2004-03-26
>     Do these metals require any kind of annealing treatments, and if so what
> are they for Ti, W, and Pt?

"require" for what? The contacts are ohmic right away, further anneals are
done to form the respective silicides or to phase-transform them. All just
to lower contact resistance.
"correct" process will depend on your junction depth.
best regards,
klaus
--
Klaus Beschorner
Metron Technology Europe, PVD (Eclipse) Process Manager
Drosselweg 6,71120 Grafenau,Germany. Tel +49-7033-45683



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Harrick Plasma, Inc.
Nano-Master, Inc.