MEMSnet Home: MEMS-Talk: Microchannel Hydrophilic problems
Microchannel Hydrophilic problems
2004-03-25
Tushar Bansal
2004-03-26
Virginia Soar
2004-03-29
Michael D Martin
Microchannel Hydrophilic problems
Michael D Martin
2004-03-29
So you have a long-ish 5 micron channel that is open only at the ends?
If that is the case there is no way the oxygen radicals will get inside.
I think the mean free path length at 100's of mTorr is around a
centimeter. You will need to use some sort of wet chemistry. I think a
strong base might work, check the literature.

-Mike


>>> [email protected] 03/25/04 4:30 PM >>>
Hello everyone,
I am trying to make a PDMS channel using PR-1827 as a sacrificial layer.

The height of the photoresist is 5 um, and then i spin a 5 um coat of
PDMS
on it. Etch away the PR and get a channel under the PDMS.

The problem I am facing is that the channel doesn't become hydrophilic
even after I put it in Oxygen Plasma. I have done 10 mins at 450 mT at
100W. The outside of the PDMS does become hydrophilic.

Am I working with too small of a channel depth or am I overlooking
something?? Do I need to treat it with Oxygen plasma for a few hours??

Please advise, as I have been stuck with this problem for
quite some time.

Thanks in advance
tushar

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation