2004-03-31
Chen-Han Lee
2004-03-31
Josef Kouba
CFD
2004-04-01
Vikas Nair
nickel based alloy for electroplating
Josef Kouba
2004-03-31
NiFe (81/19) - melting point 1450 Deg C.

Regards

J.K.

----- Original Message -----
From: "Chen-Han Lee" 
To: "Mems-Talk" 
Sent: Wednesday, March 31, 2004 1:05 PM
Subject: [mems-talk] nickel based alloy for electroplating


>
> Hi group,
>
> does any one know if any nickel based alloy can be electroplating and have
a
> high melting point(above 1500oC)??
>
> thanks in advance
>
> Chen-han
>
>
>
> ///////////////////////////////////
> Chen-Han Lee
> Research Student
> School of Manufacturing and Mechanical Engineering,
> University of Birmingham,
> Birmingham, B15 2TT
> United Kingdom,
> Phone :  +44 121 4144245
> Fax :    +44 121 4143958
> E-Mail : [email protected]
> ///////////////////////////////////
>
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
The Branford Group
MEMS Technology Review
Mentor Graphics Corporation