A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: how to remove Silicon Nitride
how to remove Silicon Nitride
2004-04-01
Qing Yao
2004-04-02
Hong Wu
2004-04-02
Loren St. Clair
2004-04-02
Blunier, Stefan
2004-04-02
William Lanford-Crick
how to remove Silicon Nitride
Qing Yao
2004-04-01
Hi,


I was wondering if H3PO4 (at between 160 to 180 degrees centigrade) can
remove Silicon Nitride without attacking Silicon Dioxide. Are there any
other methods I could use?


Best Regards,


Qing Yao
___________________
M&IE @ UIUC



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing