wet etch of Al
2004-04-02
Zannitto, Peter J.
2004-04-02
Xiaoshan Zhu
2004-04-15
hare krishna
2004-04-02
Greg Miller
2004-04-02
William Lanford-Crick
2004-04-09
[email protected]
wet etch of Al
William Lanford-Crick
2004-04-02
Try KOH.

I use 0.1 M KOH to remove 100A Al overcoat on my PMMA before
developing--it takes about 30-40 sec.  You may want to try a
higher KOH concentration for your thickness of Al, or it
will take a long time!

-Bill

---- Original message ----
>Date: Fri, 2 Apr 2004 00:23:13 -0500
>From: "Zannitto, Peter J."

>Subject: [mems-talk] wet etch of Al
>To: 
>
>
>My structure consists of 250nm PMMA / 700nm of Al / 1um
SiO2.
>
>I have done e-beam lith on the PMMA layer and developed.  I
now want to etch the Al down to the SiO2.
>
>Can anyone recommend an Al etchant that should be used in
these circumstances?  The selectivity of the etch between
the Al and the PMMA should be as high as possible.
>_______________________________________________
>[email protected] mailing list: to unsubscribe or
change your list
>options, visit http://mail.mems-
exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing
services.
>Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
MEMStaff Inc.