vijay j
oxide wet etch on ito
vijay j
2004-04-04
hai,
     you can try hf no

regarding,
vijay.

jo ed  wrote:
Hello

I have a substrate coated with ito followed by oxide.
Does anyone know of a selective wet etch process to
remove the oxide put keep the ito?

cheers,
Jo

__________________________________
Do you Yahoo!?
Yahoo! Search - Find what you’re looking for faster
http://search.yahoo.com

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/
Win an evening with the Indian cricket captain: Yahoo! India Promos.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Mentor Graphics Corporation