Hi,
I am tring to model the exposure behavior of a negtive resist. I have some
experience of modeling positive resist using the absorbing-bleaching
relationships. However, I found very limit information of modeling
negative resist in several text books. I am wondering if anyone can
suggest some literatures on this to me.

Peng Yao
DOEs lab
Electrical Engineering Dept.
Univeristy of delaware
Newark D.E 19716


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Addison Engineering