RE: Glass trench etch
Michael Marrs
2004-04-26
Lisen-

Your etch rate will probably be on the order of 0.2 microns per minute using
a fluorocarbon/oxygen mixture. You should use a chromium mask, if you have
the capability, as you will find that using photoresist will be problematic.


Michael Marrs
Process Engineer
Trion Technology
+1 (480) 968-8818 ext. 25
[email protected]



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMStaff Inc.