A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: {111}-plane mirror by KOH-etching
{111}-plane mirror by KOH-etching
2004-04-27
Armin Werber
2004-04-27
manjula raman
2004-04-28
Ashwin Seshadri
{111}-plane mirror by KOH-etching
Armin Werber
2004-04-27
Dear all,

I want to use the KOH etched {111}-planes as mirrors. In a first
experiment I used a KOH solution with following properties:
concentration: 30% KOH by weight
temperature: 85°C
magnetic stirring

The result: the roughness of the mirror planes is with about 150 nm rms
extremely high (messured with zygo white light interferometer).
I have read about the use of IPA to change the wetting properties of the
solution. (less gas bubbles adhesion on the etched surfaces)
So knows anybody the right formula for KOH-etching to achieve smooth
{111}-planes?

Kind regards,
                        Armin Werber






Institute of Microsystem Technology
University of Freiburg
Georges-Köhler-Allee 102
79110 Freiburg

Tel.: +49 761 203 7518
Fax.: +49 761 203 7562

  [email protected]
 
www.imtek.uni-freiburg.de/micro-optics


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Harrick Plasma, Inc.
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing