etch mask for KOH Etching
mahdi bagheri
2004-04-27
Hi Manjula,
You can use a low pressure chemical vapor deposition
(LPCVD) nitride or Au/Cr for deep and long KOH
etching.

Regards,
Mahdi Bagheri

manjula raman  wrote:
 I need some information of some etch mask other than
silicon dioxide for KOH etching.I am doing a long
duration etching(atleast 5 hrs)and using a thick
thermally grown oxide mask.But, the sides of my wafer
start etching out.I have tried PECVD Nitride as mask
but that does not help.Is there any resist i can apply
to the edges of my wafer during the last 1-1.5hrs of
my etching
Manjula
_______________________________________________
[email protected] mailing list: to unsubscribe or
change your list
options, visit
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS
processing services.
Visit us at http://www.memsnet.org/




__________________________________
Do you Yahoo!?
Win a $20,000 Career Makeover at Yahoo! HotJobs
http://hotjobs.sweepstakes.yahoo.com/careermakeover


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Harrick Plasma, Inc.
Mentor Graphics Corporation