Hi,

I have an issue with Cu UBM wet-etching. I use Nitric acid together with acetic
acid and hydrogen peroxide. Although my over etching time is long enough (50 to
80%) to clear all un-masked Cu, round shape Cu residue is left behind.
Does anyone know what causes this kind of residue? Any idea or suggestion will
be greatly appreciated.

Thanks & brgds,
Nang Htoi


---------------------------------
Do you Yahoo!?
Win a $20,000 Career Makeover at Yahoo! HotJobs
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
University Wafer
Mentor Graphics Corporation