We tested evaporated copper in 30% KOH at 80 C.
Rather than etching, it got thicker, indicating that some reaction was
occuring.

Remember that many etch rates have been tabulated and are available online;
see the archives for more info.

    --Kirt Williams

----- Original Message -----
From: "Tan, Chuan Seng" 
To: 
Sent: Wednesday, April 28, 2004 9:42 PM
Subject: [mems-talk] Does KOH or TMAH attack Cu ?


> Hello !
>
> Does anyone know if Si etchants like TMAH or KOH attack Cu ? If they do,
at what rate ?
>
> MANY THANKS !!
>
> CSTan
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing