A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: RIE Oxide etch - stop on gold
RIE Oxide etch - stop on gold
2004-05-05
neo man
2004-05-05
[email protected]
RIE Oxide etch - stop on gold
[email protected]
2004-05-05
neo man:

Try etching thru approximately 90% of your film and then change your power
settings to around 50 watts rf for the remaining film. Using C4F8 or CHF3 should
also help but I think you are sputter etching the gold by applying too much
power and etching too long. Do you have an endpoint system that you can use to
determine when the oxide is beginning to clear? Good luck  Bob Henderson


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
The Branford Group
University Wafer