MEMSnet Home: MEMS-Talk: GaAs/AlGaAs RIE etching
GaAs/AlGaAs RIE etching
2004-05-12
Lorenzo Sirigu
2004-05-12
Brent Garber (2 parts)
2004-05-12
[email protected]
2004-05-15
William Lanford-Crick
Photlith on transparent materials
2004-05-15
William Lanford-Crick
2004-05-16
Shay Kaplan
GaAs/AlGaAs RIE etching
Lorenzo Sirigu
2004-05-12
Hello,
I'm trying to etch by RIE very deep pillars (16 um) in a GaAs/AlGaAs
superlattice (30% Al content) with SiCl4/Cl2/Ar sources.
The result is often not very good since sometimes I have filaments with
a resulting rough surface. I've been told that one problem could be an
excess of Cl in the mixture but its reduction did not lead always to
better results.
Do you have some ideas?
Is it maybe a kind of contamination or leak in the chamber?
Thank you

Lorenzo



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Nano-Master, Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing