Tushar Bansal
2004-05-12
Hello Everyone,
I am trying to make photopatternable PDMS. I am using methacrylate
terminated PDMS and mixing it with Xylenes and DMAP (DMAP is the
photoinitiator, Xylenes is a thinner). This solution was reported in
several papers. However, it is polymerizing far too quickly and the DMAP
is not dissolving. Furthermore, on exposure and development, no actual
pattern is observed. Are we missing a step in this procedure? The amounts
of each chemical to use were not reported in the papers.

Please suggest any missing steps to the above procedure or any alternate
procedures to achieve a photo patternable PDMS.

Thanks,
Tushar


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMStaff Inc.
The Branford Group
Tanner EDA by Mentor Graphics