MEMSnet Home: MEMS-Talk: Reflectivity Drift in Sputtered Aluminum Thin Films
Reflectivity Drift in Sputtered Aluminum Thin Films
2004-05-13
PRAMOD GUPTA
2004-05-13
[email protected]
Reflectivity Drift in Sputtered Aluminum Thin Films
[email protected]
2004-05-13
this could originate from rising substrate temperature leading to bigger
grains.
Shay Kaplan

Original Message:
-----------------
From: PRAMOD GUPTA [email protected]
Date: Thu, 13 May 2004 09:55:07 -0700 (PDT)
To: [email protected]
Subject: [mems-talk] Reflectivity Drift in Sputtered Aluminum Thin Films


Does any one has experience in reflectivity drift in Sputtered Aluminum
Thin Films from 1st wafer to 25th wafer? If yes, what could be the possible
reasons for that?


(Pramod Gupta)

20800 Valley Green Dr., # 445

Cupertino, CA 95014

Phone: (408) 253-1646
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

--------------------------------------------------------------------
mail2web - Check your email from the web at
http://mail2web.com/ .




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review
University Wafer