A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: refraction index of LPCVD silicon dioxide
refraction index of LPCVD silicon dioxide
2004-05-14
Qing Yao
2004-05-14
X. Yuan
2004-05-14
Shile
2004-05-17
Feridun Ay
2004-05-14
Michael D Martin
2004-05-15
Gert Eriksen
2004-05-17
Glenn Silveira
50 +/- 5 micron through hole in Pyrex wafer
2004-05-17
Patrick Roman
2004-05-18
Zheng Xia
2004-05-18
David Nemeth
refraction index of LPCVD silicon dioxide
Feridun Ay
2004-05-17
Dear Yao,

Recent replies on the topic were all correct. The refractive index of a
typical LPCVD silicon oxide (SiOx) is around 1.46 +-0.01 (@633 nm). However,
I think that you should be careful with the growth parameters. More
precisely, the relative amounts of silicon and oxygen in your film may
deviate from ideal SiO2. If during the growth process the amount of supplied
oxygen is insufficient you can end-up with silicon rich oxide, which in turn
implies a film with a refractive index higher than 1.46. The highest
possible index in this case  is about ~2. In order to avoid this situation
you can use excess O supply during the growth (increase the precursor gas
flow rate supplying oxygen).

Regards,


Feridun Ay
Bilkent University
Ankara




-----Original Message-----
From: Qing Yao [mailto:[email protected]]
Sent: 14 May 2004 19:46
To: MEMS-talk
Subject: [mems-talk] refraction index of LPCVD silicon dioxide

Hi,


I was wondering if some one could tell me the typical value of refraction
index of LPCVD Silicon Dioxide. It is deposited at about 420 degrees
centigrade on a silicon wafer. I use a focus ellipsometer to measure its
thickness. I tried 1.46 but got very large fit error (about 500). Please let
me know if you have any information about this. Thanks!


Best Regards,


Qing Yao
___________________
M&IE @ UIUC







reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering
Mentor Graphics Corporation