MEMSnet Home: MEMS-Talk: 50 +/- 5 micron through hole in Pyrex wafer
refraction index of LPCVD silicon dioxide
2004-05-14
Qing Yao
2004-05-14
X. Yuan
2004-05-14
Shile
2004-05-17
Feridun Ay
2004-05-14
Michael D Martin
2004-05-15
Gert Eriksen
2004-05-17
Glenn Silveira
50 +/- 5 micron through hole in Pyrex wafer
2004-05-17
Patrick Roman
2004-05-18
Zheng Xia
2004-05-18
David Nemeth
50 +/- 5 micron through hole in Pyrex wafer
David Nemeth
2004-05-18
Well, CO2 lasers are out, as is ultrasonic drilling.  I don't know about RIE
or other methods, but you might look into excimer lasers - one company that
specializes in excimer laser micromachining is:
http://www.potomac-laser.com/
(They have a technology that allows for a very small spot size.)



David Nemeth
Senior Engineer
Sophia Wireless, Inc.
14225-C Sullyfield Circle
Chantilly, VA
-----Original Message-----
From: [email protected]
[mailto:[email protected]]On
Behalf Of Patrick Roman
Sent: Monday, May 17, 2004 3:36 PM
To: General MEMS discussion
Subject: [mems-talk] 50 +/- 5 micron through hole in Pyrex wafer


MEMS-talk:


What is the recommended process method to produce a 50 +/- 5 micron through
hole in a 1mm thick Pyrex wafer?  Dimensional tolerances and repeatability
are important to our design.


--

Patrick Roman, M.S.
Microsystems Engineer
Code 553- Detector Systems Branch
Room E042 Building 11
NASA/ Goddard Space Flight Center
Greenbelt,MD 20771
phone: (301) 286-3558
fax: (301) 286-1672
mobile: (202) 294-8602
email: [email protected]


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.