Hi,


I plan to use HF (or buffered HF) to do a very small amount of isotropic
etch of single crystal Silicon to remove the surface roughness after DRIE
(BOSCH process). Does anybody have a recipe (solution formula, etch rate...)
for that? Also, please let me know if there are other methods which can be
used to make the surface smoother. Thanks!



Best Regards,


Qing Yao
___________________
M&IE @ UIUC



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation