using HF to etch Si
2004-05-27
Qing Yao
2004-05-28
Neal Ricks
using HF to etch Si
Neal Ricks
2004-05-28
How slow do you want to go?  Madou notes conc. HF to have the very slow rate of
0.3A/min at 25C on n0type Silicon in the 1-1-1 direction.  If you want something
faster than that, you should apply a dilute HNA (HF+Nitric+Acetic) to the
problem.

Neal




Qing Yao  wrote:
Hi,


I plan to use HF (or buffered HF) to do a very small amount of isotropic
etch of single crystal Silicon to remove the surface roughness after DRIE
(BOSCH process). Does anybody have a recipe (solution formula, etch rate...)
for that? Also, please let me know if there are other methods which can be
used to make the surface smoother. Thanks!



Best Regards,


Qing Yao
___________________
M&IE @ UIUC


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

---------------------------------
Do you Yahoo!?
Friends.  Fun. Try the all-new Yahoo! Messenger
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics