Hello,

I have pure gold-layered silica electrodes (thin gold layer on glass)
that I would like to completely decontaminate after sensing uses, can
anyone reccomend a wet gold cleaning process that will not etch my gold
or silica.

I was recomented to use Piranah, but that does etch my gold after a
period of time.

Thank you,
Ed




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Addison Engineering