Suyong Jung
2004-06-02
Brubaker Chad
2004-06-02
Michael D Martin
2004-06-03
Bill Moffat
HMDS onto SiO2
Michael D Martin
2004-06-02
SiO2 is hydrophilic. If you prime this surface with HMDS you will see a
dramatic effect.

-Mike


>>> [email protected] 6/2/2004 2:18:57 PM >>>
Hello folks

Is there somebody who knows the way to check the quality of HMDS coated
on
SiO2.
 From the knowledge that I've collected so far, normally people try a
contact angle method, but
, as you know, SiO2 is also hydrophobic just like HMDS is.
I would like to check the qualify of HMDS, and the completeness of HMDS

monolayer coating onto the wafer as well.

Thanks in advance

Suyong




_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk

Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Addison Engineering
MEMStaff Inc.
Process Variations in Microsystems Manufacturing