Metal Question
2004-06-08
Tripp, Marie Kathleen
2004-06-08
Rick Morrison
2004-06-08
Borski, Justin
Metal Question
Borski, Justin
2004-06-08
Hello,

You may have trouble, as HF etches Alumina, so you are getting undercut of
your film, no matter what the metal is that you try to use.

Also, if you are depositing Chromium onto Alumina using a liftoff process,
you are probably using evaporation with no sputter etch of the substrate;
adhesion for that approach usually will be less than sputter-deposition
preceded by a sputter etch insitu.

You might try the sputter deposition with a pre-etch using Chromium and then
photo followed by an Ion Beam Etch, and resist strip.  But your metal
pattern will still be undercut by HF if it is sitting on top of Al2O3.

- Justin

Justin C. Borski
MEMS Program Manager
Advanced MicroSensors Inc.
[email protected]





-----Original Message-----
From: Tripp, Marie Kathleen [mailto:[email protected]]
Sent: Tuesday, June 08, 2004 12:41 PM
To: General MEMS discussion
Subject: [mems-talk] Metal Question


Hi Everyone,  I was wondering if someone could suggest a metal which will
adhere to Alumina and can be patterned with liftoff and will survive (at
least for a while) in HF?  I tried Chromium but was unsuccessful.  I
throught that I'd ask before I tried too many other metals.

Thanks,
Marie

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

**********************AMS CONFIDENTIAL AND PROPRIETARY
INFORMATION*****************************
This e-mail communication and any attachments are confidential and intended only
for the use of the designated recipients named above.



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Harrick Plasma, Inc.
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics