Cedric,

A good article to refer to on SU-8 bonding would be as follows:

S.K. Sampath, L.St.Clair, Xingtao Wu, D.V. Ivanov, Q. Wang, C.Ghosh, and
K.R.Farmer, "Rapid MEMS Prototyping Using SU-8, Wafer Bonding and Deep Reactive
Ion Etching,: Proceedings of the 14th Biennial University/Government/Industry
Microelectronics Symposium, Richmond, VA, June 17-20, 2001 - IEEE Catalog No.
01CH37197

This article specifically deals with the bonding of patterned SU-8 to an etched
silicon substrate.

Best Regards,

Chad Brubaker

EV Group       invent * innovate * implement
Technology - Tel: (602) 437-9492, Fax: (602)437-9435 e-mail:
[email protected], www.EVGroup.com

This message and any attachments contain confidential or privileged information,
which is intended for the named addressee(s) only. If you have received it in
error, please notify the sender immediately and then delete this e-mail. Please
note that unauthorized review, copying, disclosing, distributing or otherwise
making use of the information is strictly prohibited.

 -----Original Message-----
From:   [email protected] [mailto:mems-talk-
[email protected]]  On Behalf Of Cédric margo
Sent:   Thursday, June 10, 2004 12:49 AM
To:     [email protected]
Subject:        [mems-talk] SU8-silicon bonding

Hello,
 I want to make a microfluidic chip for biological analyses. The chip
would be made like this:
A SU8 layer is patterned by lithography onto a glass wafer to form a
channel and reservoirs(typically, dimensions are 20µm*20µm for the
smallest part of the channel).
After that, a silicon wafer through etched (KOH) to form fluidic and
electrical connexions would be bonded to the SU8 layer by heating of
this last.

I have still doubts about this step. So, I would appreciate any
suggestion or related links about bonding of SU8 on silicon after the
SU8 has been patterned by UV exposition.

Best regards


--
Cédric Margo - [email protected]
Laboratoire d'Instrumentation Electronique de Nancy
Faculté des Sciences et Techniques
Boulevard des Aiguillettes - BP 239
54506 Vandoeuvre les Nancy - FRANCE
Tel:03 83 68 41 56
fax:03 83 68 41 53
http://www.lien.uhp-nancy.fr



_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Addison Engineering
Process Variations in Microsystems Manufacturing
University Wafer