A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: How to make an SEM sample?
How to make an SEM sample?
2004-06-09
Josef Kouba
2004-06-09
Jon Hiller
2004-06-11
Josef Kouba
2004-06-11
Isaac Wing Tak Chan
2004-06-09
Campe, Steve
2004-06-10
Tripp, Marie Kathleen
2004-06-11
Josef Kouba
2004-06-11
Mac McReynolds
2004-06-11
Borski, Justin
How to make an SEM sample?
Josef Kouba
2004-06-11
Hi Marie,

thanks a lot for your advice, but it would not work in my case I guess.. the
sample is only supposed to be about 20 um thick and the resist hight is over
1 mm. even if I would manage to cut the wafer with 20 um precision, cleaving
it after with 1 mm resist on top of it would be impossible.

Any other suggestions? there must be a way how to do it, there are so many
samples which have to be investigated such a way and they are often even
more tough and larger that mine..

J-

----- Original Message -----
From: "Tripp, Marie Kathleen" 
To: "General MEMS discussion" 
Sent: Thursday, June 10, 2004 9:13 AM
Subject: RE: [mems-talk] How to make an SEM sample?


> Hi Josef,
>
> I like to use a saw to pre-scribe wafers which I want to break later on.
I use a normal dicing saw but only cut partially through the wafer on the
backside.  Then do my normal spinning, etc. for photo-litho.  When I want to
break the wafer later on the fracture lines are already defined.  I like
this technique because all of the mess and heat of dicing is done with
before any of the photo-litho.
>
> Cheers,  Marie
>
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
University Wafer
Tanner EDA by Mentor Graphics
MEMStaff Inc.