MEMSnet Home: MEMS-Talk: Coating issue
Coating issue
2004-06-19
chong hanwoo
Coating issue
chong hanwoo
2004-06-19
Hi,

Recently I'm concerning about a few coating issues and hope everyone can shed
some lights on these. The coating was done using e-beam evaporator, the issues
are

1. For a tri-layer film structure (SiO2-Al-SiO2) on glass substrate, the edges
of the sample started to become 'cloudy'or 'hazzy' after a 1 month. But this
'cloudiness' can be wiped off using alcohol.

2. For a multilayer TiO2 and SiO2 coating, when the sample was cleaned by using
a cleaning wiper with chemical Silicone/alcohol, the surface of the coating
started to show 'scratch' lines parallel to the cleaning direction.

Any idea on the cause and/or solution to these issues is appreciated.

Han



____________________________________________________________
Find what you are looking for with the Lycos Yellow Pages
http://r.lycos.com/r/yp_emailfooter/http://yellowpages.lycos.com/default.asp?SRC
=lycos10

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
Harrick Plasma, Inc.
Nano-Master, Inc.