MEMSnet Home: MEMS-Talk: corner compensation structure for 100 Si in KOH
corner compensation structure for 100 Si in KOH
2004-06-21
Nibras Sahib Awaja
2004-06-23
Michael L
corner compensation structure for 100 Si in KOH
Nibras Sahib Awaja
2004-06-21
Dear all,
I am trying to add a compensation structure to the convex corner of <100>Si
spring and etch it in KOH+water. Could you please advice me about how can I
choose the right dimension of these structure.
Cheers,
Nibras

-----Original Message-----
From: [email protected]
To: [email protected]
Date: Mon, 21 Jun 2004 02:00:51 +1000 (EST)
Subject: MEMS-talk Digest, Vol 20, Issue 22

Send MEMS-talk mailing list submissions to
        [email protected]

To subscribe or unsubscribe via the World Wide Web, visit
        http://mail.mems-exchange.org/mailman/listinfo/mems-talk
or, via email, send a message with subject or body 'help' to
        [email protected]

You can reach the person managing the list at
        [email protected]

When replying, please edit your Subject line so it is more specific
than "Re: Contents of MEMS-talk digest..."




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Harrick Plasma, Inc.
The Branford Group