Dear all,

I'm thinking of making tapered structure on SU-8. SU-8 usually gives a very
good vertical structured component. However, I wanted to make SU-8 structure
to be taper with a certain degree of angle, say 45 degrees. Has anyone ever
try making such structure using SU-8?

Thanks.
Abang Annuar Ehsan
Photonics Tech. Lab
Institute of Micro Engineering and Nanoelectronics (IMEN)
Universiti Kebangsaan Malaysia (UKM)
---
Outgoing mail is certified Virus Free.
Checked by AVG anti-virus system (http://www.grisoft.com).
Version: 6.0.698 / Virus Database: 455 - Release Date: 6/2/2004


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
University Wafer
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation