MEMSnet Home: MEMS-Talk: Dry Etch of Platinum
Dry Etch of Platinum
2004-06-22
Wizards Handicapping
2004-06-22
William Lanford-Crick
Dry Etch of Platinum
William Lanford-Crick
2004-06-22
A quick search at Engineering Village turned up the following
suggestions:

  Dry etching of platinum films with TiN masks in an Ar/O2
helicon wave plasma
Chiang, Ming-Chung (Natl Nano Device Lab); Pan, Fu-Ming;
Cheng, Han-Chung; Liu, Jeng-Shu; Chan, Shih-Hsiung; Wei, Ta-
Chin Source: Journal of Vacuum Science and Technology, Part
A: Vacuum, Surfaces and Films, v 18, n 1, Jan, 2000, p 181-
187

Platinum etching using a TiO2 hard mask in an O2/Cl2/Ar plasma
Chung, Chee Won (Samsung Advanced Inst of Technology); Chung,
Ilsub Source: Journal of Vacuum Science and Technology, Part
A: Vacuum, Surfaces and Films, v 18, n 3, May, 2000, p 835-839

Etching of platinum thin films by high density Ar/Cl2/HBr
plasma
Kim, C.-I. (Chungang Univ); Kim, N.-H.; Chang, E.-G.; Kwon,
K.-H.; Yeom, G.-Y.; Seo, Y.-J. Source: Materials Research
Society Symposium - Proceedings, v 514, Advanced
Interconnects and Contact Materials and Processes for Future
Integrated Circuits, 1998, p 357-362

Study on fence-free platinum etching using chlorine-based
gases in inductively coupled plasma
Chung, Chee Won (Samsung Advanced Inst of Technology); Song,
Ho Gun Source: Journal of the Electrochemical Society, v 144,
n 11, Nov, 1997, p L294-L296
Database: Compendex


---- Original message ----
>Date: Tue, 22 Jun 2004 09:24:19 -0400
>From: "Wizards Handicapping" 
>Subject: [mems-talk] Dry Etch of Platinum
>To: 
>
>   Hi:
>
>
>
>   Does anyone know of a parallel plate RIE method for
>   etching platinum, along with some potential masking
>   layers?  It can be F or Cl based.  I haven't been
>   able to find much information on it, if anyone has a
>   reference or some suggestions it would be much
>   appreciated.
>
>
>
>   Thanks
>
>   Omar.
>
>   [email protected]
>
>
>
>
>________________
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change
your list
>options, visit http://mail.mems-
exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing
services.
>Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
MEMS Technology Review