optical properties of silicon
Kirt Williams
2004-06-22
According to D.E. Aspenes, in Properties of Crystalline Silicon, p. 683,
for intrinsic silicon at 1.55 um (0.80 eV), alpha = 0.000 cm-1.
That's zero absorption, to several figures, at that wavelength.
The table lists non-zero absorption below 0.20 eV and above 1.00 eV.
    --Kirt Williams

----- Original Message -----
From: "Sachin Tyagi" 
To: 
Sent: Tuesday, June 22, 2004 11:57 AM
Subject: [mems-talk] optical properties of silicon


>
>  hi
>  i am looking for the value of absorption coefficient of silicon at 1.55
> microne,so if any body can help me,i will be very thank full to him,
>
> thanks to all
> wating for postive reply from any one
>
>
>  sachin tyagi
> indian institute of technology
> madras(chennai),india
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
The Branford Group
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics