Hi,

I fabricated SU8 on the Si substrate and printed PDMS using SU8 as a
molder.When PDMS layer was peeled off from SU8 molder some PDMS which was
not fully solidified adsorbed on Si. How can I clean the residua and
repeated use the SU8 molder?


Laura W


mems-talk-
[email protected]µÄÐżþÄÚÈÝ:

> Send MEMS-talk mailing list submissions to
>       [email protected]
>
> To subscribe or unsubscribe via the World Wide Web, visit
>       http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> or, via email, send a message with subject or body 'help' to
>       [email protected]
>
> You can reach the person managing the list at
>       [email protected]
>
> When replying, please edit your Subject line so it is more specific
> than "Re: Contents of MEMS-talk digest..."



Wu Lei


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
The Branford Group
Mentor Graphics Corporation