photoresist remove
2004-06-28
Yilei Zhang
2004-06-28
Shile
2004-06-28
[email protected]
photoresist remove
Shile
2004-06-28
A fluorescence microscope is good for detecting resist residue.

Roger Shile

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Yilei Zhang
Sent: Monday, June 28, 2004 12:54 PM
To: [email protected]
Subject: [mems-talk] photoresist remove

Hello all:
If using photoresist as mask material, sometimes we need to make sure
that no
photoresist left on the area that will be etched. is there any way to
make sure
all exposed photoresist are removed after developing? thanks.

Regards,
Yilei Zhang
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
University Wafer
The Branford Group