polyimide etching
Bill Moffat
2004-06-29
Bob,
    Good to see you are still active on the web.  You are right about the
addition of CF4 one of our customers is using 30% CF4, 70% O2, running hot near
270 degrees C and removing 8 microns of hard baked Polymide in 4 minutes.  Bill
Moffat

-----Original Message-----
From: [email protected] [mailto:[email protected]]
Sent: Tuesday, June 29, 2004 7:59 AM
To: General MEMS discussion
Subject: Re: [mems-talk] polyimide etching


Try adding some CF4 to you oxygen. This will help to remove some of the filler
material which is contained in Polyimides. It doesn't always give a clean etch
but it works for most imides. Bob Henderson
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
University Wafer
Process Variations in Microsystems Manufacturing