Problem in Lift-off process...
2004-06-28
VELHA Philippe 054082
2004-06-29
hare krishna
Problem in Lift-off process...
hare krishna
2004-06-29
Hi Philippe,
                 Do you have any idea that one should increase the temperature
of the substrate during deposition of Ni/Au on p-GaN and if yes then how much or
it should be done at room temperature...

Sincerely
Hare







VELHA Philippe 054082  wrote:
I also do lift off process on no-doped GaN but I think it should be the same
thing.
To answer your question, I think you don't put enought resist on the sample
before spin coating.
I had the same problem, there is resist only on the center of the sample.
If you have tiny samples, like me ( 5mm*5mm)
Try to do that : put your sample on something else like a glass wafer or a
silicon one or something else just to stick on it.
use your resist as a glue, post baking some second.
Spin coat, but put enought resist to overcover your sample and a part of
your support wafer.
It's not sure it works but I do that and the lift off works
An other thing, be sure of the thickness of the resist layer
PS: for information my procedure is
1) cleaning wafer like you
2)spin coating a positive photoresist (S1818) at 3000 rpm for 10s
3) post bake for 2 min at 110°C
4) exposure
5)develop with MF 319 30s

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

Yahoo! India Matrimony: Find your partner online.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
Tanner EDA by Mentor Graphics
University Wafer