MEMSnet Home: MEMS-Talk: P-metal
P-metal
2004-07-07
[email protected]
P-metal
[email protected]
2004-07-07
Hello,
We have a Ti+Pt+Au  metalized  laser wafer. The stripe direction is wrong.
Any idea how we can etch off this metalization? The wafer was annealed @
420C for  1min.
Thank you

Peter Tihanyi
PLT Technology, Inc
Phone# 805-685-7449