Hi,Kirt Williams:

  Do you need to bake the polyimide before you do wet etching? Another question
is,will photoresist work as well as chromium?

  Thanks a lot.

Ping Zhang




==============

>We've tried a number of etchants for PI 2556, which I will guess is similar.
>Piranha worked, but is too fast.
>Microstrip 2001 (a commercial photoresist stripper), at 85 C, etched at
>about 0.5 um/min.
>You would have to use a hard mask such a thin layer of chromium.
>    --Kirt Williams
>
>----- Original Message -----
>From: 
>To: "mems-talk" 
>Sent: Wednesday, July 14, 2004 4:19 PM
>Subject: [mems-talk] Polyimide Wet Etch
>
>
>> Could anyone give me a recipe for wet etching polyimide (PI2555)? I tried
>several ways but nor worked.
>>
>> Thanks
>> - ware.
>>
>>
>>
>> _______________________________________________
>> [email protected] mailing list: to unsubscribe or change your list
>> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>> Hosted by the MEMS Exchange, providers of MEMS processing services.
>> Visit us at http://www.memsnet.org/
>
>
>

= = = = = = = = = = = = = = = = = = = =





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
MEMStaff Inc.
MEMS Technology Review