MEMSnet Home: MEMS-Talk: How can I improve the attachment of SU-8 to PDMS?
How can I improve the attachment of SU-8 to PDMS?
2004-07-20
X J
How can I improve the attachment of SU-8 to PDMS?
X J
2004-07-20
Dear colleague,
  Is there any way to improve the attachment of SU-8 to PDMS? I want to use
SU-8 and PDMS to create double layers. But the attachment is always not
good enough. I used the plasma treatment.
  Thank you.


  Sincerely,
  Jason