A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Double depth SU-8
Double depth SU-8
2004-08-16
Matthew Davies
2004-08-17
newman
Double depth SU-8
Matthew Davies
2004-08-16
Hi all

I’m trying to find out if there is an easy method for seeing developed
SU-8 through another layer of SU-8.  We are trying to make devices
requiring double depth processing and the aligning of the photomask for
the second layer is very difficult as we are currently unable to see the
developed SU-8 on the bottom layer.  At the moment we need to
overdevelop the bottom SU-8 layer until cracks appear at which point we
can see the cracks through the top layer of SU-8.

Any suggestions would be much appreciated.

Thanks all

Matt Davies
STRC, University of Hertfordshire

---
Outgoing mail is certified Virus Free.
Checked by AVG anti-virus system (http://www.grisoft.com).
Version: 6.0.738 / Virus Database: 492 - Release Date: 16/08/2004


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering
Mentor Graphics Corporation