Ebeam lithography on glass substrates
2004-08-17
Francois Montaigne
2004-08-17
William Lanford-Crick
Ebeam lithography on glass substrates
William Lanford-Crick
2004-08-17
Hello Francois,

I have had no trouble doing ebeam lithography on glass when I coat the PMMA
with 10 nm Aluminum.  You have 10 nm metal under the PMMA--that should be
fine if the metal is fairly conductive (if not, try putting 10 nm Al on TOP
of the PMMA--it is easy to strip off in KOH prior to developing the PMMA).
I have used 50 kV and 100 - 250 pA beam current.  Proximity effects, in my
case, were not any different than on a silicon substrate.

With the metal on TOP of the PMMA, I can make an electrical contact from
that metal to the sample holder of the ebeam system using a metal clip.  In
your case, you may not have any electrical contact between your metal and
the sample holder.  Try using a metal coating on top of the PMMA (in
addition).

Good luck,
Bill Lanford-Crick

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Francois Montaigne
Sent: Tuesday, August 17, 2004 10:31 AM
To: [email protected]
Subject: [mems-talk] Ebeam lithography on glass substrates


Hi,
We are currently trying to do Ebeam lithography on metallic layers (about
10 nm thick). We use PMMA resist and 30 keV electron energy. Whereas we
obtain good results with silicon substrates (18-30 ohm.cm), the patterns
are dramatically rounded on glass substrates. Can it be du to a dramatic
proximity effect on glass? We rather suspect that some charges are trapped
in the substrate despite the conductive metallic layer between the
substrate and the resist. Does some of you have any experience with Ebeam
lithography on glass or insulator substrates or can advise any reference on
that subject?
Regards
Francois

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMStaff Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review