MEMSnet Home: MEMS-Talk: Tin Oxide Etching Process
Tin Oxide Etching Process
2004-08-27
[email protected]
2004-09-06
David Nemeth
Tin Oxide Etching Process
[email protected]
2004-08-27




Hi !!!!!!!

Please Suggest me the Chemicals and Wet Etching Process For Tin Oxide
Coated Glass. My glass Plate size is
1200 mm x 700 mm and Sputter Coated Tin oxide Thickness is 1.6 Micron.

Nadig Pranesh