MEMSnet Home: MEMS-Talk: RIE process of LSMO/LSMO manganite film
RIE process of LSMO/LSMO manganite film
2004-08-30
Suyong Jung
RIE process of LSMO/LSMO manganite film
Suyong Jung
2004-08-30
Dear all,

I'd like to check if there is any way to do patterning onto LSMO ( LCMO )
manganite film. I've come to know RIE would be possible to make manganite
electrodes exclusively, but struggled to find which types of gases and
parameters should be used.
If you let me know any reference paper or information about the process, it
would be wonderful for me, and if there might be different ways to
fabricate manganite patterns without RIE process, please let me know.

Best Regards,

Suyong


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering