MEMSnet Home: MEMS-Talk: The color of poly or amorphous silicon deposited PECVD?
The color of poly or amorphous silicon deposited PECVD?
2004-08-31
Kasman , Elina
2004-08-31
Phillipe Tabada
2004-09-01
WALTER Harald
The color of poly or amorphous silicon deposited PECVD?
Kasman , Elina
2004-08-31
The fact that you have nitrogen present during the deposition certainly
means that you will have certain mixture of it in the film. How much you
don't know unless you do some kind of spectral analysis. Why not use
pure silane?

Elina

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Jinkee Lee
Sent: Monday, August 30, 2004 8:11 PM
To: [email protected]
Subject: [mems-talk] The color of poly or amorphous silicon deposited
PECVD?


Hi all,



I deposited Si on glass using PECVD, but I am wondering it is really Si
or Si nitride.

Our Silane source is 2% SiH4 mixed with N2. So, I supplied SiH4 and N2.

With my deposition, the color was yellow with thin layer and getting red
with thick layer.



If someone has a same experience, please let me know.

Thanks



Jinkee Lee

Brown Univeristy, Division of Engineering

Ph.D. student@Microfluidics Lab, Tripathi Group.

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
The Branford Group
Mentor Graphics Corporation