Wet Etch ITO Coated Glass
Borski, Justin
2004-08-31
Tim,

You can try 17% HCL to etch ITO films, try to keep your etchant at constant
temp, maybe 25 degrees +/- 1 degree.  A resist mask of any positive-tone
variety will work, S1813, AZ4400, etc.  Etch rate should be somewhere around
30-60 Ang/min, which is pretty slow.

- Justin

Justin C. Borski
MEMS Program Manager
Advanced MicroSensors Inc.
[email protected]



-----Original Message-----
From: Krueger, Bernd (Unaxis Optics BZ)
[mailto:[email protected]]
Sent: Tuesday, August 31, 2004 3:57 AM
To: 'General MEMS discussion'
Subject: AW: [mems-talk] Wet Etch ITO Coated Glass


Hello Tim,

Once I have tried etching ITO on Glas with NH4HF2 and it works, but the Glas
will also etched. Unfortunately the etched regions on the substrate became
matt.

Bernd Krueger

-----Ursprüngliche Nachricht-----
Von: [email protected]
[mailto:[email protected]]Im Auftrag von Kinney, Tim Scott
(UMC-Student)
Gesendet am: Dienstag, 27. Juli 2004 04:52
An: [email protected]
Betreff: [mems-talk] Wet Etch ITO Coated Glass

I am interested in wet etching ITO coated glass for a research project I am
involved in.  I am looking specifically for products and a procedure to wet
etch ITO coated float glass.  Since the pattern I will be using does not
require high definition, I will be using a printed transparency as my mask.
I will have access to spin coating equipment as well.  I have been told the
basics, but I have had a hard time finding specific information about  what
kind of resist, developer, and solvent to use.  Any information will be very
helpful and appreciated.

Thank you,
Tim
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

**********************AMS CONFIDENTIAL AND PROPRIETARY
INFORMATION*****************************
This e-mail communication and any attachments are confidential and intended only
for the use of the designated recipients named above.



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Addison Engineering
The Branford Group
Mentor Graphics Corporation