MEMSnet Home: MEMS-Talk: RF MEMS Capacitive Switch Fabrication
RF MEMS Capacitive Switch Fabrication
2004-09-01
karthikeyan shanmugavelu
RF MEMS Capacitive Switch Fabrication
karthikeyan shanmugavelu
2004-09-01
hi all,


 I am doing my work on design and development of RF MEMS Capacitive switch. For
that I optimised the layout in an EM Simulator (Intellisuite) . Next I am going
to fabricate the same. Here I need the guidance about what all are the materials
involved and Process Flow for fabricate the switch.

The guidance I expect you is may be some Books, transactions, journals or any
websites deal the Process Flow.

Thanks in advance,


S.Karthikeyan,
Project Associate,
Thiagarajar College of Engg.,
Madurai,
India.



On Mon, 30 Aug 2004 [email protected] wrote :
>Send MEMS-talk mailing list submissions to
>       [email protected]
>
>To subscribe or unsubscribe via the World Wide Web, visit
>       http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>or, via email, send a message with subject or body 'help' to
>       [email protected]
>
>You can reach the person managing the list at
>       [email protected]
>
>When replying, please edit your Subject line so it is more specific
>than "Re: Contents of MEMS-talk digest..."
>
>
>Today's Topics:
>
>    1. equipartion theoram (rakesh babu)
>    2. wet etch that etches Al but not ZnO (Raegan Johnson)
>    3. MF 351 or AZ 351 (Joolien Chee)
>
>
>----------------------------------------------------------------------
>
>Message: 1
>Date: Sat, 28 Aug 2004 21:45:44 -0700 (PDT)
> From: rakesh babu 
>Subject: [mems-talk] equipartion theoram
>To: [email protected]
>Message-ID: <[email protected]>
>Content-Type: text/plain; charset=us-ascii
>
>Folks,
>
>  Does anyone have an idea regarding equipartion energy and its relation to the
thermal noise in cantilevers.
>
>regards
>rakesh
>
>Peter Svasek  wrote:
>Hi,
>
>SILICON RESOURCES (www.siliconresources.com) offer an adhesion promoter
>(AP 300) for SU-8
>on glass.
>Did you try slow temperature ramps during PEB ? your problem might also
>be caused by stress because of
>the high CTE of SU-8.
>
>Best regards
>Peter
>
>--
>Vienna University of Technology
>Institute of Sensor and Actuator Systems
>Gusshausstrasse 27-29/366
>A-1040 Wien
>Austria
>
>Tel. +43-1-58801-36643
>Fax +43-1-58801-36699
>
>
>
>
>Arne Schleunitz wrote:
>
> >Hi,
> >
> >I have adhesion problems of 120um thick and 50um wide SU-8 50 structures on
pyrex.
> >I have a long dehydration time (at least one hour), a high exposure dose
(600mJ/cm2) and even tried stepwise exposure.
> >Although I could improve the adhesion some parts still peel of during the
development.
> >I know, that by increasing the exposure dose I could get better adhesion, but
an unwanted side effect would be rough sidewalls that I try to prevent...
> >
> >I appreciate any comments!!! Thanks in advance.
> >
> >Arne
> >
> >---
> >
> >Arne Schleunitz
> >
> >MEMS Sensors and Actuators Lab
> >
> >Department of Electrical and Computer Engineering
> >
> >University of Maryland
> >
> >Tel: (301) 405-1897
> >
> >_______________________________________________
> >[email protected] mailing list: to unsubscribe or change your list
> >options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> >Hosted by the MEMS Exchange, providers of MEMS processing services.
> >Visit us at http://www.memsnet.org/
> >
> >
> >
>
>
>
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/
>
>
>---------------------------------
>Do you Yahoo!?
>Yahoo! Mail Address AutoComplete - You start. We finish.
>
>------------------------------
>
>Message: 2
>Date: Sun, 29 Aug 2004 13:51:08 -0500 (CDT)
> From: "Raegan Johnson" 
>Subject: [mems-talk] wet etch that etches Al but not ZnO
>To: [email protected]
>Message-ID: <[email protected]>
>
>Does anyone know of a wet etch solution that will etch aluminum but not ZnO?
>
>thanks,
>Raegan
>
>
>
>
>------------------------------
>
>Message: 3
>Date: Sun, 29 Aug 2004 21:57:27 -0500
> From: Joolien Chee 
>Subject: [mems-talk] MF 351 or AZ 351
>To: [email protected]
>Message-ID: <[email protected]>
>Content-Type: text/plain; charset=US-ASCII; format=flowed
>
>Hi all,
>
>I would like to know what is the difference between Microposit MF 351
>and Shipley AZ 351. The target photoresist is Shipley 1813.
>
>Thank you all in advance.
>
>Joolien
>
>
>
>------------------------------
>
>_______________________________________________
>MEMS-talk mailing list
>[email protected]
>http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
>
>End of MEMS-talk Digest, Vol 22, Issue 26
>*****************************************

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
The Branford Group
Tanner EDA by Mentor Graphics