Kim, Ick Chan
Looking for adhesives between Au(200nm) and polymer film(20nm)
Kim, Ick Chan
2004-09-05
Dear MEMs researcher,

I need to deposit Au(200nm) on the coated polymer film(20nm), but in order
to stick Au on the polymer film safly, what mateial can make it between Au
and polymer film?   Chrome can be adhesives between Au and silicon, but I
don't know what can be between Au and polymer film.
Thank you very much.

Sincerely
Ickchan Kim


--
Ickchan Kim                              Office Phone: (979)845-9598
[email protected]                           C.P.#       : (979)574-4179

Office: ENPH #401, Conduction Heat Transfer Lab.
        Department of Mechanical Engineering, Texas A&M University
        College Station, Texas 77843-3123





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
MEMStaff Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing