Dear All

Hello.
I am looking for the process condition of Au/Sn(20) eutectic bonding.
I found that the melting point of Au/Sn(20) alloy is 278℃. But I could not
find
how large pressure is required on bonding process.

If you have any information on Au/Sn bonding. please give me some
information.

Thanks for your help.

S.H. Choe

Esashi-laboratory, Faculty of Engineering,
Tohoku university, Sendai, Japan

[email protected]



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
The Branford Group