MEMSnet Home: MEMS-Talk: Problem about making 1mm thickness su-8 micromold
Problem about making 1mm thickness su-8 micromold
2004-09-10
tida
Problem about making 1mm thickness su-8 micromold
tida
2004-09-10
How to make this kind of thick mold?
Is that the procedures similar to normal case? ( like spin coating
>>softbake >> uv exposure >> hard bake >> develope.....)
And what kind of su-8 should i choose? su-2000?


What is the meaning of multi spinning programme?

"With a multi spinning program, we have patterned in one exposure a
1200 µm and a 2300 µm layer, which is, to our knowledge, the thickest
structure ever patterned using microfabrication techniques."  by IBM
( http://dmtwww.epfl.ch/ims/micsys/projects/su8/epon.html )

Does anyone make a such thick mold before?
Can you share your experience?

Any of suggestions and advice are valuable to me.
 thanks in advance.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
MEMStaff Inc.
The Branford Group