A 10:1 BOE solution for 15 seconds should be enough to remove native oxide on
silicon. Under normal circumstances there can be from 8-25 angstroms of native
oxide prior to removal by HF. If possible after DI water rinse it would be
better to dry using an isopropyl alcohol drying system and immediately go to
your sputtering system. If your sputtering system also has an RF clean station
prior to deposition you can Argon clean using that station prior to dep. Bob
Henderson

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
University Wafer
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing